Easy Fashion Metal Products Co., Ltd.

Easy Fashion Metal Products Co., Ltd Your Advanced Powder Metallurgy Expert

Manufacturer from China
Active Member
8 Years
Home / Products / Powder Manufacturing Equipment /

Magnetic Powder Metallurgy Manufacturing Process For Amorphous Alloy Powder Production

Contact Now
Easy Fashion Metal Products Co., Ltd.
City:changsha
Province/State:hunan
Country/Region:china
Contact Now

Magnetic Powder Metallurgy Manufacturing Process For Amorphous Alloy Powder Production

Ask Latest Price
Video Channel
Brand Name :Easyfashion Industry
Model Number :EFZKT-50
Certification :CE Certificate
Place of Origin :China
MOQ :1 set
Payment Terms :T/T, D/A, D/P, Western Union
Supply Ability :10 sets per year
Delivery Time :120 days
Packaging Details :standard export wooden cases or containers
Common heating temperature :1200°C
Feeding Material :10-3 Pa
Leakage volume :less than 10-9Pam3/sec
Smelting capacity :5~50g/based on iron;
Highest heating temperature :1500°C
Injection pressure :max. 0.1MPa
more
Contact Now

Add to Cart

Find Similar Videos
View Product Description

200 KG Fast Amorphous Alloy Powder Production Equipment For Iron Base Nanometer Material

Overview

Amorphous Alloy Powder Production Equipment is the magnetic material processing equipment that continuously produces amorphous alloy powders by using high-speed cooling method. The large-scale production is conducted under protective gas or vacuum condition. The produced powders are mainly used for electrics, electronic components, military industry etc..

Specifications

  • High-frequency output: 5kW;
  • Smelting capacity: 5~50g/based on iron;
  • Cooling roller rotating speed: 100-500rpm (single roller size: Φ200*20mm);
  • Vacuum reaching pressure: 10-3 Pa (when filling with specimen and nozzle);
  • Highest heating temperature: 1500°C;
  • Leakage volume: less than 10-9Pam3/sec;
  • Output frequency: 100KHz.
  • Injection pressure: max. 0.1MPa;
  • Common heating temperature: 1200°C;
  • Power supply: 3 phases, 220V, 13KVA (clients need to prepare voltage transformer for their own)
  • Cooling water: 25L/min, water pressure: 0.35MPa (backpressure: less than 0.1MPa)

Inert gas (Ar): displaced capacity 100L/per time, pressure 0.5MPa.

Features

Its working principle refers to that smelted metal is jetted onto quench cooling roller in high-speed rotation under given conditions in Ar gas environment after vacuum exhausting, and then the amorphous thin band is formed though quench cooling process.

Inquiry Cart 0